TECHNET Archives

September 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Date:
Sun, 11 Sep 2011 21:01:10 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Kane, Joseph E (US SSA)" <[log in to unmask]>
Message-ID:
Subject:
From:
"Kane, Joseph E (US SSA)" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (127 lines)
Thanks Joyce.  We have such batch systems, and we'll be trying to get them back on line.

-Joe

________________________________________
From: TechNet [[log in to unmask]] On Behalf Of Joyce Koo [[log in to unmask]]
Sent: Sunday, September 11, 2011 7:22 PM
To: [log in to unmask]
Subject: Re: [TN] Cleaning Up After The Flood

There are dishwasher type of semi aquas cleaner for electronics.  It high jetting and drying may help.  But 1st, a good brush with DI may need to get rid majority of mud.  Good luck.  My 1 cent.
--------------------------
Sent using BlackBerry


----- Original Message -----
From: Bob Landman [mailto:[log in to unmask]]
Sent: Sunday, September 11, 2011 05:08 PM
To: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] Cleaning Up After The Flood

Joe,

That's an incredibly sad story.  My sincere condolences.

Hmm... perhaps Dove for dishes which is what is used to clean wildlife that's been caught in oil spills.

We use a diliute solution of trisodium phosphate for precleaning boards we are electrolessly plating with nickel - that leaves no soapy residue and removes oil films.

Compressed air or nitrogen is a good idea to get rid of excess water but be careful of induced static electricity in the air stream.
See. for example http://www.iprocessmart.com/Exair/static_eliminators.htm

Be very careful for your health as that water isn't just muddy river water, it likely contains coliform bacteria from failed waste treatment plants that dumped into the river.

Bob
  _____

From: Kane, Joseph E (US SSA) [mailto:[log in to unmask]]
To: [log in to unmask]
Sent: Sun, 11 Sep 2011 15:14:39 -0400
Subject: [TN] Cleaning Up After The Flood

Tropical Storm Lee dumped about 9 inches of rain on Binghamton, and we got the second hundred-year flood in five years.  But this one was lots worse than in 2006.  Cities and towns were inundated, and a lot of people have lost their homes here.  And this time the Susquehanna River overtopped the levee and flooded our plant.

  The water has receded and we were able to send people inside yesterday to assess damage.  A lot of our product is wet and muddy, from components on reels on up to finished assemblies.  And essentially all of our assembly and test equipment has been at least partly submerged.

  Not sure if we can get some of our cleaning equipment restored soon, including aqueous batch dishwashers and an in-line aqueous cleaner.  If we have to clean product in buckets or tubs, we're thinking about these steps:

  1. Soapy/alkaline water solution, scrub as necessary
  2. At least two rinses, last one DI
  3. Blow off with compressed air (or nitrogen if available)
  4. Bake
  5. Ionic contamination testing on samples

  Our conformal coat is mostly urethane.  Some assemblies have unsealed connectors, switches, and pots.  Some motherboard/front panel assemblies have lots of wires.

  Anybody have any experience cleaning river mud from electronics?

  Joe Kane
  BAE Systems
  Johnson City, NY

  ______________________________________________________________________
  This email has been scanned by the MessageLabs Email Security System.
  For more information please contact helpdesk at x2960 or [log in to unmask]
  ______________________________________________________________________

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 16.0
  To unsubscribe, send a message to [log in to unmask] with following text in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
  Search the archives of previous posts at: http://listserv.ipc.org/archives
  For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
  -----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2