TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 27 May 2005 11:07:05 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Vladimir Igoshev <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Vladimir Igoshev <[log in to unmask]>
Parts/Attachments:
text/plain (80 lines)
I always enjoy when Werner "praises" the shear test. :-) From what I know, the only case it might be really useful is to check whether the components could be "blown off" and I don't mean a case of poor wetting. I don't know the root cause (hopefully yet), but it could happen with ENIG finished boards (and it WOULDN'T be a case of either Black Pad or Brittle Fracture!!!!!).

Regarding a correlation between having a proper wetting and good solder joints, it's may be not a  straight forward thing. Potentially, we may have a good wetting (at least on ENIG boards, just because the wetting behavior, which is just spreading the solder along the surface, would be defined by the presence of Au) but poor solder joints (no proper intermetallic layer was formed for some reason). 

Vladimir

Research in Motion
451 Phillip St.
Waterloo, ON, N2L 3X2

Voice: (+1) 519-888-7465, ext. 5283
Fax: (+1) 519-886-0863
E-mail: [log in to unmask]


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Werner Engelmaier
Sent: Thursday, May 26, 2005 7:19 PM
To: [log in to unmask]
Subject: Re: [TN] IMC and Wetting


 Hi Brad,
I did indeed.
Nothing much has changed with SAC solders in this respect. The IMCs will be still with Sn and the base metal. There is no optimum thickness.
Shear strength is not a useful metric for SJ quality--with SJs it is a  step-function, either you have proper wetting or you no not. What is important is not the shear strength, but the failure mode: it is either brittle interfacial [that means when you look at the 2 fracture surfaces they do NOT have the same metallurgy], or ripped out soldering pads [fractures in the SJs are indeed very rare] indicating good 'wetting' and a strong metallurigical bond. Your reflow profile is ditto an all-or-nothing proposition: either all SJs are properly 'wetted' or some of them [in the center of BGAs] saw insufficient heat. Do not fall for this non-technical advice of 60 to 90 seconds above 183C--this does not assure proper wetting. You need Liquidus+20C [Liquidus+35C when soldering to Ni] for at least 5 seconds for even the slowest heating SJ to assure 100% good quality SJs.
Werner Engelmaier

-----Original Message-----
From: [log in to unmask]
To: [log in to unmask]
Sent: Thu, 26 May 2005 16:05:37 -0500
Subject: IMC and Wetting


Werner,

In a previous Global SMT & Pkg column "Solder: Quality and Reliability
Issues" you indicated "proper wetting is the process of forming a
metallurgical bond between the base metal of the solder pad and at least
one constituent of the solder alloy, in most cases tin."  We would like to
apply this principle in determining wetting criteria for SnAgCu alloys.
Can you share any guidelines or point us to references for optimizing IMC
during assembly? (both thickness and constituents).  Do you consider shear
strength of as built PWA components to be a useful metric for comparing
variables (reflow profile, solder flux, etc)?

I realize you are very busy and I would appreciate any input you can share.

Thank you,
Brad Green, Engineer
Seagate Technology
Shakopee, MN
952-402-2451

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2