TECHNET Archives

1995

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipchq.com (Smail3.1.28.1 #2) id m0szRiH-0000H8C; Sun, 1 Oct 95 11:58 CDT
Old-Return-Path:
<[log in to unmask]> <miso!aol.com!DSober>
Date:
Sun, 1 Oct 1995 11:12:48 -0400
Precedence:
list
X-Loop:
Message-ID:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/1261
TO:
Return-Path:
Resent-Message-ID:
<"rzbgF1.0.LE5.DYiRm"@ipc>
Subject:
From:
Resent-From:
Resent-Sender:
From [log in to unmask] Sat Apr 27 14:
55:18 1996
Parts/Attachments:
text/plain (14 lines)

Dear Technet User,

I am looking for technical information concerning aramid woven and nonwoven
base materials for printed wiring board applications.  Anyone who has
information concerning fabrication of these types of laminates and prepregs
into printed boards and is willing to share their experiences both good and
bad should contact me at [log in to unmask] or by phone at 803-224-5831.

Doug Sober 