Surface nodules are caused by;
1) Excess or erratic current during electroplating
2) Contaminates in the plating solution
3) Contaminates on the work surface
to name a few...
As for is it acceptable or not, yes, there is nothing specific written about
this in IPC 6012 / A 600; however, para 1.9 Workmanship does address defects
agreed upon between supplier/customer.
Surface nodules for the most part are a process indicator, unless they are
extremely large and prone to breaking off exposing substrate...they are
unsightly and this 'visual' defect is how it is written here (at my
facility).
If your specific customer will not accept the nodules (interestingly enough
some actually have no problem with this condition) then they are cause for
reject.
There are many conditions we observe that are not directly addressed in IPC
documents...and this is where weighing all these factors from and internal
(your facility) viewpoint as well as an external (customer requirements,
needs, expectations, etc) viewpoint should all play a part in the decision
making...
Hope this helped some...
Franklin D Asbell
----- Original Message -----
From: "Schleman, Joe A." <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, December 09, 2004 9:34 AM
Subject: [TN] Plating nodules
TechNet,
We have received some pwbs that have some irregularities in the copper
plating. The board vendor is referring to these irregularities as "surface
plating nodules".
I have found information in IPC-A-600 regarding nodules in plated-through
holes but no information concerning nodules on surface traces. Can anybody
provide
any information regarding "surface plating Nodules"?
Thanks
Joe Schleman
Harold Beck & Sons Inc.
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|