TECHNET Archives

December 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 3 Dec 2004 08:46:20 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Subject:
From:
R Sedlak <[log in to unmask]>
Content-Type:
text/plain; charset=us-ascii
In-Reply-To:
MIME-Version:
1.0
Comments:
DomainKeys? See http://antispam.yahoo.com/domainkeys
Parts/Attachments:
text/plain (22 lines)
Al:  Assume the change to Silver has cured the problem?

Immersion Tin can be a bit of a problem to rinse, as it tends to gel when cooled.  We advise our customers to have a heated (warm) first rinse, which makes this problem go away.

Rudy Sedlak
RD Chemical Company


---------------------------------
Do you Yahoo!?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
 Send a seasonal email greeting and help others. Do good.

ATOM RSS1 RSS2