TECHNET Archives

October 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Elensky, Richard" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 2 Oct 2001 11:27:10 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (80 lines)
Provided physical specs of the component will accommodate the wave solder
environment (flux, heat, immersion in molten solder...) they should survive
with no problem.

We currently reflow and wave our devices without issue.

Solder pallets are another possible solution.

Happy to expand on either, off line.

Call with questions.

Richard Elensky
Sr. Manufacturing Engineer
[log in to unmask] <mailto:[log in to unmask]>

Tel:  559-292-1111  x246
Fax:  559-292-9355

Dantel
2991 North Argyle Ave.
Fresno, CA, 93727
Visit our web site at:
http:// www.dantel.com <http://www.dantel.com>


        ----------
        From:  Jorge Rodriguez [SMTP:[log in to unmask]]
        Sent:  Tuesday, October 02, 2001 10:29 AM
        To:  [log in to unmask]
        Subject:  [TN] Tantalum Caps

        Technetters,

        I have a product that has Tantalum Caps, having them waved would
make our
        life easier, the board has some TH components we currently hand
solder and
        that could be waved. I know that there might be some reason not to
wave
        Tantalums, but I am not sure. Can Tantalum Caps be wave soldered?,
Has
        anyone done this?

        Any responses would be appreciated

        Jorge Rodriguez
        Process Engineer
        Varian Inc


----------------------------------------------------------------------------
-----
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
        Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315

----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2