TECHNET Archives

July 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Ian Boyton <[log in to unmask]>
Date:
Tue, 20 Jul 1999 01:52:17 PDT
Content-Type:
text/plain; format=flowed
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Ian Boyton <[log in to unmask]>
Parts/Attachments:
text/plain (107 lines)
It would be worth having your pcb supplier measure the plating thickness,
too thin and you see soldering problems.

Best Regards

ian

>From: Francis Lai <[log in to unmask]>
>Reply-To: "TechNet E-Mail Forum." <[log in to unmask]>,        Francis Lai
><[log in to unmask]>
>To: [log in to unmask]
>Subject: Re: [TN] Sloder bubbles on the VIAs
>Date: Wed, 14 Jul 1999 21:49:08 -0700
>MIME-Version: 1.0
>From [log in to unmask] Fri Jul 16 08:27:09 1999
>Received: from [209.42.15.76] by hotmail.com (2.0) with ESMTP id
>MHotMailB9589A47003DD82197E2D12A0F4CC50C0; Fri Jul 16 08:27:09 1999
>Received: from jefry ([209.42.15.79])by mail.ipc.org (8.8.8+Sun/8.8.8) with
>ESMTP id JAA12587;Fri, 16 Jul 1999 09:54:31 -0500 (CDT)
>Received: from IPC.ORG by IPC.ORG (LISTSERV-TCP/IP release 1.8d) with spool
>id          2020189 for [log in to unmask]; Wed, 14 Jul 1999 20:38:29 -0500
>Received: from mail.ipc.org (209.42.15.76:39570) by IPC.ORG (LSMTP for
>Windows          NT v1.1b) with SMTP id <[log in to unmask]>; Wed, 14 Jul
>1999          20:38:29 -0500
>Received: from freenet.carleton.ca (freenet1.carleton.ca [134.117.136.20])
>by          mail.ipc.org (8.8.8+Sun/8.8.8) with ESMTP id UAA16725 for
>    <[log in to unmask]>; Wed, 14 Jul 1999 20:47:33 -0500 (CDT)
>Received: from freenet.carleton.ca (p13t3.std.dialup.ncf.carleton.ca
>   [134.117.137.172]) by freenet.carleton.ca (8.9.1a/8.9.1/NCF_f1_v3.00)
>       with ESMTP id VAA09878; Wed, 14 Jul 1999 21:46:54 -0400 (EDT)
>X-Mailer: Mozilla 4.61 [en] (Win95; I)
>X-Accept-Language: en
>References:
><[log in to unmask]>
>Message-ID:  <[log in to unmask]>
>Sender: TechNet <[log in to unmask]>
>X-To:         "Tempea, Ioan" <[log in to unmask]>
>
>"Tempea, Ioan" wrote:
>
> > Hi,
> >
> > now that the problem with the blistering solder mask is fixed ( we sent
>the
> > boards back since backing them was of no use), I have another one.
> >
> > Some of our assemblies have a high density of VIAs. On these products,
> > pretty often we get after wave some solder bubbles over the VIAs, some
>of
> > them exploded, like degassing. Since on some we see the same bubbling
>even
> > on the fiducials, I wonder if the humidity is the only one to blame, I
>even
> > wonder if there's any issue related to humidity at all.
> >
> > So, what could it be? Incompatibility between flux and solder sounds
> > possible?
> >
> > I would appreciate any input,
> >
> > Ioan
>
>Dear Ioan :
>
>To me it sounds like copper plating problem. The surface of the base copper
>probably was not cleaned enough, it caused blisters. I think if you do a
>tape
>test after copper plating, probably, copper plated will peel.
>
>Please correct me if I am wrong!!!
>
>Francis
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in
>the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
>additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################


______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2