Edwin,
There is basic information available at
http://nepp.nasa.gov/whisker/background/index.htm
While Tin whiskers can still occur when using conformal coating but the use
of coating can help minimize the problem.
Bill Kasprzak
Moog Inc., Systems Group, Process Engineer
-----Original Message-----
From: David Suraski [mailto:[log in to unmask]]
Sent: Monday, July 26, 2004 10:36 AM
To: [log in to unmask]
Subject: Re: [TN] Tin Whiskers
From what I have heard (and please don't ask where I heard it), the
short answer is NO - the whisker will grow right through the coating.
And the same goes for acrylics and silicones. I've heard that paralenes
may be better.
Regards,
David Suraski
AIM
+1-401-463-5605 ext. 5210
www.aimsolder.com
-----Original Message-----
From: Edwin Louis [mailto:[log in to unmask]]
Sent: Monday, July 26, 2004 10:20 AM
To: [log in to unmask]
Subject: [TN] Tin Whiskers
Does anyone know whether a Polyurethane conformal coating would inhibit
Tin whisker growth or at least contain it?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|