Sender: |
|
Subject: |
|
From: |
|
Date: |
Thu, 10 Jun 1999 08:15:54 -0500 |
Content-Type: |
text/plain |
MIME-Version: |
1.0 |
Reply-To: |
|
Parts/Attachments: |
|
|
John,
You may want to look into the Loctitie VariDot stencil
technology. It is a flexible plastic film stencil that is used with
acrylic blades. By defining the snapoff height, it can create dot
heights for components from 0402 to SOICs all in the same print stroke.
We had experimented with it here a while back with successful results,
just haven't really had an application requiring it yet. The only
drawback is that they are fabricated at the Loctite facility in Ireland,
so your turn will be a couple of days to a week. Loctite will evaluate
your requirements and tailor the apertures for you based on their
knowledge of how the stencil responds. Give them a call and see what
they can do....
Mike McMonagle
PCA Process Engineering Supervisor
K*Tec Electronics
1111 Gillingham Lane
Sugar Land, TX 77478
(281) 243-5639 Phone
(281) 243-5539 Fax
[log in to unmask]
> -----Original Message-----
> From: John Chandler [SMTP:[log in to unmask]]
> Sent: Wednesday, June 09, 1999 8:55 AM
> To: [log in to unmask]
> Subject: [TN] Gluing components
>
> We have a simple board in which we are using our screen printer to
> apply
> reflow curing glue, in between the pads, etc.
>
> The chipshooter components 0603, sots, etc do perfectly.
>
> The IC's and any other part with a gull wing, J wing type do not have
> enough glue to even touch the bottom of the parts. Because as you
> know, the
> body sits off the board
>
> Step stencil comes to mind but never done that YET. Using rubber
> squeegees
> on printer. Tried putting in a big snapoff where it would leave a
> space
> between the pcb and stencil but this helps but not a cure. Any
> suggestions.
>
> Step stencil, stencil thickness. Did not put what thickness of what
> stencil
> we use to see what you all have to say.
>
> Thanks in advance.
>
> John
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|