Hi Joe,

You asked, "Can anyone recommend a southern California consultant that
could help us transition to another cleaning agent?"  I recommend to you
Ed Popelarski of QTA Machine.  Ed is in Southern California, and, is an
industry consultant with many years of process and equipment experience.
More specifically for your needs, he has worked with various cleaning
suppliers in a multitude of capacities.  Ed is based in Mission Viejo,
CA and can be reached at 949-581-660.

Best Regards,

Shean Dalton
Austin American Technology
512-335-6400 ext. 20

                        ------Original Message-----
                        From: Macko, Joe @ IEC
                        Sent: 5/26/2004 2:53 PM
                        To: [log in to unmask] <mailto:[log in to unmask]>
                        Subject: [TN] Replacement for Ecosolve
Saponifier


                        Good Morning,

                        Another potential line stopper has appeared on
the horizon. My production
                        supervisor notified me that the Ecosolve
saponifier made by AlphaMetals is
                        no longer available. We have a WESTEK in-line
cleaner that uses Ecosolve to
                        clean RMA flux residue from boards. We are also
located in Southern
                        California so we have stringent drainage and air
quality (VOC emission)
                        rules that need to be considered.

                        Does anyone have any excess EcoSolve they would
like to sell to get us
                        through this transition?

                        Has anyone faced this same problem and switched
from EcoSolve to another
                        aqueous cleaner to remove RMA flux residue and
no clean?

                        AlphaMetal's is recommending their ARMAKLEEN
E-2003 as a replacement for
                        Ecosolve. Anyone out there using ARMAKLEEN that
would like to comment on
                        its performance on RMA (and no-clean)?

                        Can anyone recommend a southern California
consultant that could help us
                        transition to another cleaning agent?


                        thanks
                        joe


---------------------------------------------------
                        Technet Mail List provided as a service by IPC
using LISTSERV 1.8e
                        To unsubscribe, send a message to
[log in to unmask] with following text in
                        the BODY (NOT the subject field): SIGNOFF
Technet
                        To temporarily halt or (re-start) delivery of
Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
                        To receive ONE mailing per day of all the posts:
send e-mail to [log in to unmask]: SET Technet Digest
                        Search the archives of previous posts at:
http://listserv.ipc.org/archives
                        Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315

-----------------------------------------------------



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2