TECHNET Archives

November 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"McMonagle, Mike" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 21 Nov 2000 14:41:55 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (67 lines)
                Patty,
                        Check out http://www.ccrco.com/ for ESD safe
micro-blast equipment

                Mike McMonagle
                Senior SMT Engineer
                Telxon Corporation

                                -----Original Message-----
                                From:   Goldman, Patricia J.
[mailto:[log in to unmask]]
                                Sent:   Tuesday, November 21, 2000 1:57 PM
                                To:     [log in to unmask]
                                Subject:        [TN] micro sand blasting

                                Technet colleagues,

                                My boss came across the term "micro sand
blasting" in an article in the
                                April 2000 edition of SMT Magazine.

                                He asked me what that was and of course I
did not have an answer.  Can
                                someone give me a nice description of this
operation or process?

                                The article had to do with Conformal
Coatings and the pertinent sentence
                                was:  "Rework on acrylics and urethanes can
be handled using mechanical
                                abrasion or micro sand blasting."

                                Thanks for your help,
                                Patty
                                Patricia J. Goldman
                                PPG Industries, Inc.
                                724-274-3417
                                [log in to unmask]


----------------------------------------------------------------------------
-----
                                Technet Mail List provided as a free service
by IPC using LISTSERV 1.8d
                                To unsubscribe, send a message to
[log in to unmask] with following text in
                                the BODY (NOT the subject field): SIGNOFF
Technet
                                Search previous postings at: www.ipc.org >
On-Line Resources & Databases > E-mail Archives
                                Please visit IPC web site
(http://www.ipc.org/html/forum.htm) for additional
                                information, or contact Keach Sasamori at
[log in to unmask] or 847-509-9700 ext.5315

----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2