> Dear All,
>
> Recently, we found a very strange defect with the BGA IC.
>
> Here's our process flow: SMT---> De-panel (by V-cut machine)--->
> Functional test--->final inspection
>
> We found around 10 pcs BGA falling out either at the process of de-panel or
> functional test, defect rate less than 0.1%. The defect only happened in 2
> days, It's very strange, all the solder balls adhere to PCB. there's no
> solder ball adhere to the BGA substrate.
>
> Investigations from our side:
> 1. We have been built the same product since April 2004. no issue before.
> 2. Since May 2005, the SMT process was converted to RoHS, BGA also has been
> changed to green type since then, monthly output around 200K.
> 3. The BGAs were 100% baked under 110 degreeC for 24 hrs before SMT.
> 4. We use Loctite LF318 solder paste for SMT, the time between 70 degreeC
> to peak 245 degreec is around 250 seconds.
> 5. The BGA only subjected to 1 time reflow (only 1 side with components)
> 6, We have reflow fixture to support the board during reflow. there's no
> warpage issue.
> 7, Use Vcut machine to separate the units from a 6 up-panel PCB, no extra
> stress to the board.
> 8. Use pogo pin to make connection for functional test fixture, no extra
> stress.
>
> Information of BGA.
> 1. It's a solder mask defined substrate. with ENIG surface finishes.
> 2. 0.8mm pitch, pad size 0.35mm.
> 3. IC supplier apply solder ball with flux only, without solder paste.
>
> Would anybody give me some advices, what shall be the most possible root
> cause? it's a BGA IC issue or a SMT process issue? How to improve?
>
>
> Thanks
> Willis Tam
>
>
>
>
>
>
>
>
>
>
>
>
>
>
>
>
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|