Hi Matthew! We are currently evaluating on-site N2 generation versus
cryogenic sourcing hence my question last week. We are currently using
cryogenic nitrogen (purity 99.99%) in both our wave solder and SMT
soldering applications. Our internal testing results shows that a oxygen
ppm range of 100-300 in the "reflow segment" of the reflow oven increases
the process robustness for component pitches less than 20 mil. And there is
increasing industry data showing that nitrogen increases the Pbfree
soldering process envelope. Good Luck.
Dave
Matthew Park
<MPark@PRECO-MORT To: [log in to unmask]
ON.COM> cc:
Sent by: TechNet Subject: [TN] Another Nitrogen Purity Question/Survey
<[log in to unmask]>
03/17/2004 10:00
PM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to
Matthew Park
Hi all cryogenic heads,
Several years ago, I looked into a membrane nitrogen generator for the
possibility of supplying inert gas for reflow ovens and wavesoldering
machines.
Are companies using N2 generated by the membrane N2 technology for
reflow/wave? If so, what N2 purity level can be generated?, And how
successful is it for inerting electronic assembly applications?.
Who are major players for supplying membrane nitrogen generators?
thanks
Matthew
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|