TECHNET Archives

February 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stephen R. Gregory" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 2 Feb 2000 13:55:44 EST
Content-Type:
text/plain
Parts/Attachments:
text/plain (45 lines)
In a message dated 02/02/2000 12:35:26 PM Central Standard Time,
[log in to unmask] writes:

<< I'm a little confused.  J-STD-013 recommends 22 mil pads for 1.00mm pitch
 BGAs, but the guideline for IPC7527 suggests 15 mil round pads with a square
 paste opening.  Is anyone out there having good luck with one or the other?
 Why the large disparity?

 Thanks-

 > Larry Jindra
 > TRW/Avionics Systems Division
 > mailto:[log in to unmask]   ph (858) 592-3424   fax (858) 592-3606 >>

Hi Larry!

I just finished building a prototype board yesterday that had a 256-ball
microBGA that had .020" pads, and I had my stencil apertures made into .020"
squares my stencil was 4-mils thick, and I had all the other larger apertures
left at 1-to-1 (I usually get a 20% reduction) to make-up for the loss of
volume that the 4-mil stencil is giving me. Worked great! The square aperture
will release the paste easier than a round pad that small, and it'll give ya'
a little bit of "slop factor" for placement too...as long as the balls are in
the paste, the part will self-center during reflow. I will say that the
fillets on some of my larger ceramic chip caps (1812's) were a tad bit shy
with the 4-mil stencil (least my inspectors didn't like them) but everything
else looked okay. Maybe next time I'll go up a mil to a 5-mil stencil and
make em' look better...

-Steve Gregory-

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2