I echo David's "lowest bidder" comment. Some years ago on another planet,
we bought male and female connectors to the same BS spec for a job. Each
type was bought by a different purchasing officer - one older and more
experienced, the other younger and more keen to be seen to be getting the
best price for things.

From the experienced purchaser, who asked what the real requirements were
for the job, bought in "Rolls Royce" Hypertac connectors with round, gold
plated contacts, while the less experienced fellow bought in cheapo Souriau
connectors with square, "pressed tin" contacts of very dubious reliability.
Both met the BS spec, yet the performance of the two when mated was
non-existant - virtually no inter-contact area, wide tolerences on the
Souriau's and disimmilar metals were the obvious problems. We had to scrap
all the Souriau's and buy more Hypertac's instead.

So be careful when simply buying to spec. In the eyes of a spec, all parts
are equal, but some prove to be more equal than others!

Peter



"Crepeau, Phil" <[log in to unmask]>    19/09/2002 01:09 AM
Sent by: TechNet <[log in to unmask]>

Please respond to "TechNet E-Mail Forum."; Please respond to "Crepeau,
Phil"

              To:  [log in to unmask]
              cc:  (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
              Subject: Re: [TN] Contact Plated Finish








i would like to say 'amen' to this.  unless you think living on the edge is
some kind of virtue.

phil

-----Original Message-----
From: David Douthit [mailto:[log in to unmask]]
Sent: Tuesday, September 17, 2002 5:25 PM
To: [log in to unmask]
Subject: Re: [TN] Contact Plated Finish


Victor,

Dissimular metals used for contacts is very seldom a good idea.

The "lowest bidder" concept, in this case, could result in catastrophic
failures.

Gold to gold is, particuarly for power contacts, is by far and away the
best match!

David A. Douthit
Manager
LoCan LLC

Victor Hernandez wrote:

> Fellow TechNetters,
>
>    Does anyone known if this combination of plated surfaces will create a
> problem.
>                         Male Pin                                Female
pin
>         1).  Contact pin:  base material/Nickel/Tin     Contact Pin:
base
> material/silver
>
>   application on a power connector.
>
> Victor,
>
>
---------------------------------------------------------------------------------

> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
>
---------------------------------------------------------------------------------


---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------


---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------





[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2