TECHNET Archives

October 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Tempea, Ioan" <[log in to unmask]>
Date:
Tue, 18 Oct 2005 07:58:58 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Stephen R Gregory <[log in to unmask]>
Subject:
From:
Stephen R Gregory <[log in to unmask]>
X-cc:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (78 lines)
                                I have yet to experience (that I know of), any failures due to
                                voiding. We have done thermal cycling (no vibe) on a few
                                assemblies that have BGA's, but no HALT.

                                Haven't assembled anything with BGA's with a water soluble
                                flux, we use no-clean (Indium SMQ-92J).

                                Kind regards,

                                -Steve Gregory-
                                Senior Process Engineer
                                LaBarge Incorporated
                                Tulsa, Oklahoma
                                (918) 459-2285
                                (918) 459-2350 FAX





        "Tempea, Ioan" <[log in to unmask]>
                        Sent by: TechNet <[log in to unmask]>
                        10/18/2005 07:31 AM
                        Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to "Tempea, Ioan" <[log in to unmask]>
                                	
        To:     [log in to unmask]@SMTP@Exchange
        cc:     (bcc: Stephen R Gregory/LABARGE)
        Subject:        Re: [TN] Voids in BGAs, again	


                                Concur with Richard,

                                good document, professional and academic. But if I am not mistakening, it does not mention real failures from voiding.

                                BTW, your experience is very well appreciated, extreme conditions, bad voids. I am wondering if regular testing, like HALT and the others caused joints to fail due to voiding.

                                What about failures due to chemistries, WS flux entrapped into voids that corrode their way out?

                                Best regards,
                                Ioan

                                > -----Original Message-----
                                > From: TechNet [SMTP:[log in to unmask]] On Behalf Of Stadem, Richard
                                > Sent: Tuesday, October 18, 2005 8:14 AM
                                > To:   [log in to unmask]
                                > Subject:      Re: [TN] Voids in BGAs, again
                                > 
                                > Thank you Steve! 
                                > This is an excellent and informational document. Thank you for posting
                                > it. 
                                > 
                                > 

                                ---------------------------------------------------
                                Technet Mail List provided as a service by IPC using LISTSERV 1.8e
                                To unsubscribe, send a message to [log in to unmask] with following text in
                                the BODY (NOT the subject field): SIGNOFF Technet
                                To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
                                To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
                                Search the archives of previous posts at: http://listserv.ipc.org/archives
                                Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
                                -----------------------------------------------------



                                __________________________________________________________________
                                This message may contain information that is privileged and confidential to LaBarge, Inc.  It is for use only by the individual or entity named above.  If you are not the intended recipient, you may not copy, use or deliver this message to anyone.  In such event, you should destroy the message and kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2