TECHNET Archives

September 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Amol Kane (Asteelflash,US)" <[log in to unmask]>
Date:
Wed, 19 Sep 2012 15:41:15 -0400
Reply-To:
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Subject:
From:
Robert Kondner <[log in to unmask]>
Content-Type:
text/plain; charset="iso-8859-1"
In-Reply-To:
Organization:
Index Designs
MIME-Version:
1.0
Parts/Attachments:
text/plain (152 lines)
Amol,

 Good Questions, I will find out.

Thanks,
Bob K.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Amol Kane
(Asteelflash,US)
Sent: Wednesday, September 19, 2012 3:30 PM
To: [log in to unmask]
Subject: Re: [TN] Broken Vias

Were the boards moisture baked before assembly? .....is the stackup
balanced? Is the via damage more pronounced in the area of warpage?


Amol Kane
Process Engineer
AsteelFlash US East Corp
Tel:   (607) 687.7669 x349 (O)
www.asteelflash.com


ITAR Confidentiality Notice: This e-mail and any attachments are
confidential. It is intended for the recipient only. Prior to forwarding
this e-mail or opening any attachments please note that they may contain
security sensitive, proprietary, or export restricted information. Any
unauthorized disclosure, use, dissemination, or copying is strictly
prohibited and may be unlawful. Furthermore, this communication may contain
technical information that is subject to U.S. Export Control Laws, including
the International Traffic in Arms Regulations (ITAR) or the Dept. of
Commerce Export Administration Regulation (EAR). If so, transfer to a
foreign national or representative of a foreign government or interest, even
in the U.S., without prior Government authorization is prohibited and
violation of such Export Control Laws is subject to significant penalties.
If you received this e-mail in error, please immediately notify the sender
by replying to this e-mail and delete the e-mail and all copies from your
computer. Although the sender and Asteelflash have taken every reasonable
precaution, the e-mail and attachments may have some errors or omissions and
may contain viruses. We cannot accept liability for any damage that you
sustain as a result of that


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
Sent: Friday, September 14, 2012 5:02 PM
To: [log in to unmask]
Subject: Re: [TN] Broken Vias

Hi,

 Does anyone know about the TCE of via plug material? I am trying to get a
material number of what was used. This was the first board we ever ran with
via plugging but I would think that is a well-known process?

Bob K.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jason Zhao
Sent: Friday, September 14, 2012 12:52 PM
To: [log in to unmask]
Subject: Re: [TN] Broken Vias

Bob,

Xsection will show you where the opens occur. Possibilities are: copper
plating folds; thin copper; corner crack; post separation; separation due to
no wraparound; etc. Then we can determine the root causes from there (there
are too many to guess now). Looking forward to some pictures.

Best Regards

Jason Zhao
VP of North America Operations
Sunshine Circuits
3400 Silverstone Drive, Suite 139, Plano, TX 75023 US Cell 510-468-4412,
China Cell 131-62722392 www.sunshinepcbgroup.com

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
Sent: Friday, September 14, 2012 10:18 AM
To: [log in to unmask]
Subject: [TN] Broken Vias

Hi,

 

A small company in the area has a board with two very expensive parts, about
$3K each part. They built 30 boards and had lots of open via connections.
They are getting cross sections now on some bad vias. In addition to many
bad vias there was some board warp. Sorry I don't have any hard numbers on
bad via counts or warp.

 

These were 10 mil holes in .062 material, a 6:1 aspect ratio, should be
easy. Vias were plugged and plated so they could be used as flying probe
test points. 

 

After reflow assembly the boards were run on a wave machine using a mask
where about 25% of the board was exposed to the wave. Everything lead free. 

 

Question:

 

Can folks suggest lists of items we can check, measure or inquire into? Any
guesses or ideas as what might be going on?

 

Thanks,

Bob K.



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2