TECHNET Archives

March 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
Date:
Tue, 12 Mar 2002 09:04:27 +0800
MIME-Version:
1.0
X-To:
Earl Moon <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (104 lines)
Passivated Nickel? Have your boards been allowed to dry out too much at
fabrication between plating stages? Boards should still be we going from
the Nickel bath to the Gold bath to minimise oxidation of the Nickel
surface, to which you're soldering (or trying to).

Peter



                    Earl Moon
                    <[log in to unmask]        To:     [log in to unmask]
                    M.COM>               cc:     (bcc: DUNCAN Peter/Asst Prin Engr/ST
                    Sent by:             Aero/ST Group)
                    TechNet              Subject:     Re: [TN] ENIG AND NON WETTING
                    <[log in to unmask]
                    ORG>


                    03/11/02
                    07:57 PM
                    Please
                    respond to
                    "TechNet
                    E-Mail
                    Forum.";
                    Please
                    respond to
                    Earl Moon






Daan,

As always, I appreciate your input. To clarify, the boards were freshly
received from a major international supplier. I instructed our assembly
house (the same major international supplier - how about that for strategic
planning as the same boards, in volume will be, guess what, assembled by
the
same major international supplier in another location) to reflow and wave
solder the solder samples. The supplier wave soldered the side in which I
had little interest. It was the SMT side, with all the little bastard TI
CSP's that held the most interest for obvious reasons or that should have
been obvious to all as it's all I've been yacking about for two months to
you all and all prospective suppliers.

I got the wave results last week with the non wetting as I described. The
wave solder process was "normal" to the major international assembly
operation with flux type, flux application, conveyor speed, wave types,
wave
height, preheat temps, solder temp, and all the other stuff we all know and
love about wave soldering and its process management requirements.

The board showed, clearly, non wetting on some bottom side SMT pads, at
about 50% non wetted. It also showed, clarly through hole pads about 50%,
by
quantity, non wetted with some obviously adhacent.

My question, again, is what in the ENIG, over bare copper after SM
application, is possibly affecting this type solderability. It's a mystery
worth more investigation.

Again, thanks Daan and I hope I clarified.

Earl

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------





[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2