TECHNET Archives

October 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 19 Oct 2004 19:31:33 EDT
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Steve Gregory <[log in to unmask]>
Parts/Attachments:
text/plain (40 lines)
Hi All!

Dave Hillman so kindly sent me a picture of some LCCC solder joints after
thermal cycling
after 500 thermal cycles of -55C to +125C (per IPC-9701 guidelines).
Needless to say it has failed! (CAUTION! Parental discretion is advised before
viewing!) Go to:

_http://www.stevezeva.homestead.com_ (http://www.stevezeva.homestead.com)

Look at: "LCCC after thermal cycling"

I build assemblies using LCCC's here, 32-pins or lower...mostly radar
stuff...been putting them on assemblies for as long as I've been  here. Don't know
exactly why our customer still uses them, maybe that's the  only package they
can get the devices in...and maybe the smaller packages don't  have the same
CTE mismatch problems.

There is a company that makes compliant SMT leads that can be attached to
LCCC components, and I think that they have a service that will do that for you.
 It's Interplex NAS, go to:

_http://www.interplexnas.com/index.asp_
(http://www.interplexnas.com/index.asp)

If you absolutely have to use LCCC's, and they're bigger than 32-pins, you
might check them out.

-Steve Gregory-

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2