Gentleman,
I need the name of a company that provides a calibration service for
stage micrometers. The calibration report must provide the dimension
between lines to 5 significant digits in inches (i.e., 0.00103 inches).
The company I used in the past has discontinued this service.
Thanks In Advance,
Randy Reed
Analytical Lab, Merix Corporation
Forest Grove, OR
503.359.9300 x5-4421
randy.reed @merix.com
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|