TECHNET Archives

August 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Bert Steck <[log in to unmask]>
Date:
Thu, 16 Aug 2012 11:33:39 -0400
Reply-To:
Message-ID:
Content-Transfer-Encoding:
7bit
Subject:
From:
Robert Kondner <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
<9EDA9A3D5C9C43FF95802724E7FD1455@BertsDesktop>
Organization:
Index Designs
MIME-Version:
1.0
Parts/Attachments:
text/plain (64 lines)
Bert,

 I have been doing this Part Numbers stuff for a good 20 / 30 years. I write
a lot of software for CAD to assembly with concentration in the PCB Assembly
and SMT assembly areas.

 Contact me off line as I would probably bore most folks on the list.

Quickly:

You need to consider your users and other company software systems first.
Most CAD tool library management threads have limited intelligence for
sorting, searching and interfacing with out-side system. Purchasing tolls
typically provide better, but still limited functions.

I tend to lean towards using "Abstract" numbers (Example 376892132) instead
of Functional (Example: SMR-5%-0606-5.1K) but using abstract require other
tools have good search and find interfaces. That is seldom the case.
Functional number schemes often "Fail" when different folks start using
different schemes or the initial scheme is not well planned. Either way you
end up with a mess.

Bob K.




 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bert Steck
Sent: Thursday, August 16, 2012 10:50 AM
To: [log in to unmask]
Subject: [TN] Part Number Classification System

We are establishing an internal part numbering system.

 

Request referral to  classification/category schema.

 

In the past (1980s) used EEM  catalogue.

 

Don't see it available or updated out there.  

 



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2