I have never experienced any problems using 2% silver solder. I have
used it very often for the same reasons that Bogert wishes to use it, to
prevent leaching of sintered silver traces from aluminum oxide (ceramic)
substrates. It is very effective for that purpose. When I attempted to
use standard Sn63Pb37 solder with those components, much of the sintered
silver traces would dissolve into the solder. When I performed the same
soldering with Sn62Pb36Ag2, it worked just fine.
I know many companies and CEMs use 2% Ag solder paste for all standard
soldering and report better wetting. I have yet to hear of a real
problem associated with it, other than cost. I have never heard of
corrosion issues associated with 2% silver solder.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, April 09, 2008 8:14 AM
To: [log in to unmask]
Subject: Re: [TN] Sn62 solder; any negative experience using it???
In addition to helping solder components with palladium/silver finish,
(although some may disagree with me on this), I found that a 2% silver
solder paste helps to reduce tombstoning...
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of - bogert
Sent: Tuesday, April 08, 2008 4:27 PM
To: [log in to unmask]
Subject: [TN] Sn62 solder; any negative experience using it???
April 8, 2008
Sn62 solder contains 2% silver. Have folks experienced any issues using
SnPb solder with this much silver? The historical QQ-S-571E solder spec
indicated that using Ag2.5 solder can result in corrosion issues in a
humid environment but I am not aware of any issues using Sn62 solder.
My understanding is that using 2% silver helps when soldering to ceramic
parts having palladium/silver finish.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|