TECHNET Archives

September 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Jorge Rodriguez <[log in to unmask]>
Date:
Thu, 6 Sep 2001 14:32:53 -0700
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (65 lines)
Ioan,

We have a product that pretty much fits the description of your board,
slightly thicker at 0.032, Our board has a .016" +/-.003" Web with a 30
degrees angle blade. One thing I got to tell you it's that a board that thin
with the v-score becomes a lot more flimsier. There are things you can do to
help to make the board more rigid such as additional copper thieving and
jump scoring.

As far as your questions: Yes, it's possible. But you might want to limit
the extent of the v-score and help the board rigidity with jump scoring and
adding copper thieving to the breakaways.


Jorge Rodriguez
Process Engineer
Varian Inc

-----Original Message-----
From: Tempea, Ioan [mailto:[log in to unmask]]
Sent: Thursday, September 06, 2001 2:16 PM
To: [log in to unmask]
Subject: [TN] V scoring of a 0.031" thick panel


Hi Technet,

I'm back with one more experience teaser.

Is it possible to score a FR4 panel, 0.031" thick? The scoring guide on the
site of Accusystems only covers the regular, 0.062".

If yes, any limitations?

What is the reccomended web thickness, I am looking at a panel about 4"x9",
double reflow, with the depanelizing right after the reflow.

Thanks,
Ioan

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2