TECHNET Archives

April 2018

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Tan Geok Ang <[log in to unmask]>
Date:
Fri, 13 Apr 2018 22:12:27 -0400
Reply-To:
Message-ID:
Content-Transfer-Encoding:
7bit
Subject:
From:
Robert Kondner <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Organization:
Index Designs
MIME-Version:
1.0
Parts/Attachments:
text/plain (41 lines)
As A Note I recall a discussion long ago that vacuum does not speed up water
diffusion.

Does anyone recall? The rate of diffusion was more dependent on the
concentration difference and temperature. 

Bob K.
-----Original Message-----
From: TechNet <[log in to unmask]> On Behalf Of Tan Geok Ang
Sent: Friday, April 13, 2018 9:23 PM
To: [log in to unmask]
Subject: Re: [TN] Vacuum Baking

Thanks. I am able to find it. Thanks

________________________________

From: Tan Geok Ang <[log in to unmask]>
Date: 14 April 2018 at 9:20:59 AM SGT
To: TechNet E-Mail Forum <[log in to unmask]>, Wayne Showers
<[log in to unmask]>
Subject: Re: [TN] Vacuum Baking

Hi Wayne,
Are you able to send me a copy? Thx

________________________________

From: Wayne Showers <[log in to unmask]>
Date: 14 April 2018 at 6:38:35 AM SGT
To: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] Vacuum Baking

You might want to check out this paper:
Characteristic Times of Moisture Diffusion and Bake-out Conditions for
Plastic Encapsulated Parts written by Alexander Teverovsky QSS Group,
Inc./Goddard Operations [log in to unmask]

I have emailed you a copy.  Of note is that the key temperature for any bake
out under vacuum is 58C.