TECHNET Archives

May 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 1 May 2006 16:37:09 EDT
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="UTF-8"
From:
Werner Engelmaier <[log in to unmask]>
Parts/Attachments:
text/plain (29 lines)
Hi Dale,
Unfortunately you are citing another example of junk science pobular 
knowledge. 
"...they only know that drinking water from lead pipes (or with leaded 
solders) is bad for you."
The first part refers to the Roman aqueducts that contained lead linings and 
pipes—a study I read not too long ago actually attributes the Pb-poisioning of 
the roman nobility to the fact that they drank their wine [acitic] from 
Pb-leaching vessels [Brian, please correct me if I am wrong on this]. the second 
one with the Pb-bearing solder used to solder copper water pipes is definitely a 
red herring. 
In New Jersey, the copper pipes were initially replaced with PCP pipes—these 
leach indefinitely, but what was worse, they sand blasted the Pb-containing 
paint off of highway bridges [how many kids have you seen chewing paint off of a 
highway bridge?] which of course made it air-borne and thus contaminated the 
backyards of people's houses close by.

Werner

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2