TECHNET Archives

May 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"Dehoyos, Ramon" <[log in to unmask]>
Date:
Wed, 28 May 2003 09:36:04 -0700
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (52 lines)
        One of the reasons may be that those products were packaged in high
altitude areas such Colorado ( low pressure ) and brought to one of the
coasts ( higher pressure ). The bottle is pressed in till the inside and
outside pressures are equal. A 50 gallon metal tank can implode if  it is
attached to a vacuum pumped and air  taken out.
        Regards,
        Ramon

> -----Original Message-----
> From: [log in to unmask] [SMTP:[log in to unmask]]
> Sent: Wednesday, May 28, 2003 9:55 AM
> To:   [log in to unmask]
> Subject:      [TN] why do HDPE bottles get deformed?
>
> We've all seen them, High Density Polyethylene bottles that have become
> all "sucked in", to the point where they're almost triangular.  I have
> bottles with rosin fluxes, and others with decap chemicals (Dynasolve
> products) that have done this - all in their original containers. They've
> been stored in an friendly environment, no strange temperatures or
> anything unusual.  Over the years I've seen many other products in poly
> bottles do the same.  The bottles seem to get very hard, and never recover
> their original shape.  Does anyone know what causes this?
>
> Bruce Tostevin
> Benchmark Electronics
> Hudson, New Hampshire
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2