Depends if you want to have solder mask defined pads or not.
If mask defined then a rule of thumb is to aim for the same mask aperture on the interposer.
Non mask defined ROT is to make the pad equal the minimum ball diameter so that solder joint forms around the pad sides
improving stress resistance.
Although, watch out for ball collapse, and consider what height is left if your needing to clean after reflow, and if there is
enough annulus for via in pad (if your forced down the HDI route).
Generally, the larger higher value device manufacturers will give some guidance. Altera and Xilinx have apps notes, some stuff
at Intel and IBM as well if you've got time to search.
If your using an EMS then they probably have their own preferences, best to go along with them because it's their job to stick
the bits down on the board with electric glue.
Some apps notes:
http://www.asat.com/products/library/fg1033.pdf
http://www.altera.com/literature/an/an114.pdf
The National Physical Lab in the UK also a wealth of data http://www.npl.co.uk/ on solder joint reliability including Pb free.
Here's a thought: With all this political correctness stuff prevailing (no naughty words etc), how do you folks on the sunny
side of the Atlantic get away with saying 'solder' and 'soldering' all of the time?
Best Regards
David Greig
______________________________
GigaDyne Ltd
Buchan House
Carnegie Campus
Dunfermline KY11 8PL
United Kingdom
t: +44 (0)1383 624 975
http://www.gigadyne.co.uk
______________________________
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Guy
Sent: 2005-May-10 17:59
To: [log in to unmask]
Subject: [TN] BGA Ball/Pad Size Ratio
Hello All,
I was wondering if there is some guideline for the recommended pad size for a BGA based on the component's ball size? I
have been told that it is recommended that the pad diameter be about 80% of the ball diameter, but I would like some
confirmation.
Thanks in advance,
John Guy
Surface Mount Process Engineer
diversifiedsystems, inc.
Custom Products Division
3939 W. 56th Street
Indianapolis, IN 46254-4961
Telephone: 317-299-9547, x336
Fax: 317-298-2055
E-mail: [log in to unmask]
Web: www.divsys.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with
following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send
e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC
web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at
[log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
--
Virus scanned by Lumison.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|