Dear Technetters,
Lately, we have been receiving bare boards from our supplier with some dents on the BGA Pads (ENIG Finish). The dent is plated too (no exposed Ni). What kinds of assembly defects can potentially be associated with this condition? (voiding and coplanarity post reflow comes to mind). Are there any specs that cover this kind of condition/defect? I want to reject this board but need something to stand by
I am sure that somebody else has seen this too, how was this dealt with?
Steve: I wish to post a picture of this condition, can you please direct me how to do it?
Thanks in advance,
Amol
------------
CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected from disclosure under the law. Any unauthorized review, use,
disclosure, or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail, and delete/destroy
all copies of the original message and attachments.
Thank you.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|