Dave,
I may be way off-base, but could you incorporate some of the very old, very
high temp flux used for reflow of 90-95Pb/10-5Sn into the paste - thinking
that it might not volatize completely at the lower temps? I believe that
Indium still had these fluxes a few years back. If you did this, you would
not alter the reflow profile, thereby keeping metallurgical structure the
same.
Having an SST vacuum reflow chamber at your disposal for a smallish test
coupon would be 'sweet' because you could vary the background pressure and
generate some really nasty frothy joints - and I would think, all that lays
in between. Just can not promise that you could duplicate your standard
reflow profile exactly.
Steve
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|