Larry,
You don't say where you are loosing your components. Handling prior to
wave or at the wave or a combination of both?
The best smd adhesive I ever ran was an Ashai (sp) product that used to
be sold by Multicore, but it went away when Loctite took them over. In
my shear tests on this product, I would break the solder mask loose from
the PWB or would break the 1206 test resistor before the smd adhesive
bond would break. GOOD STUFF - but I have not been able to find it
since Multicore stopping selling it, and believe me I have tried.
Good luck,
Gary Camac
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Davis, Larry
Sent: Friday, January 11, 2008 11:38 AM
To: [log in to unmask]
Subject: [TN] Bottom side SMT adhesives
Happy Friday Everyone!
We are currently stencil printing Loctite 3612 for our bottom side SMT
parts. We have trouble getting larger parts (SOL's, tantalums, etc) to
stay attached consistently. I'm just wondering what products others are
using for this process and if anyone has had the same issue.
Thanks and have a great weekend!
Larry
This message (including any attachments) contains confidential
and/or proprietary information intended only for the addressee.
Any unauthorized disclosure, copying, distribution or reliance on
the contents of this information is strictly prohibited and may
constitute a violation of law. If you are not the intended
recipient, please notify the sender immediately by responding to
this e-mail, and delete the message from your system. If you
have any questions about this e-mail please notify the sender
immediately.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|