All,
We've lately noticed a marked increase in the number of lifted chip
resistors and castellated termination resistor packs on one of our SMT
manufacturing lines. This began after we upped our reflow profile to solve
some solderability issues. When we recognized this new problem, we restored
to profile to its original settings, but we're still seeing the increased
volume of "floating" components. They're not completely tombstoned, but God
love 'em, they're trying their best to be.
Our solder prints measure as they always have, both in height and pad
coverage.
Any suggestions?
Thanks in advance,
Leland Woodall
Quality Coordinator
Keihin Carolina System Technology, Inc.
4047 McNair Road
Tarboro, NC 27886
Phone: (252) 641-6750, Ext. 2865
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|