TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Wayne Thayer <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Thayer <[log in to unmask]>
Date:
Mon, 21 May 2007 21:59:06 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (67 lines)
Hi Steve!

Kapton tape to hold it temporarily in place during assembly, then after
it is formed into final position, very carefully remove the kapton and
put some of that conformal coat you've got on it.

By the way, isn't that coating kind of thick?  I recall a discussion
about that on TechNet a few months ago wherein the thick conformal coat
appeared responsible for wrecking a CERDIP (not that I see any of those
in the picture).

Wayne Thayer



>>> [log in to unmask]  >>>
Hi All!
 
I got a rigid-flex assembly here that has multi-layer flex in it, and it
had a layer of the flex get torn while de-masking it after conformal
coating. I have a picture of the tear here:
 
http://www.stevezeva.homestead.com/files/Flex_Tear.jpg
 
As you see, the tear is on the edge and away from any conductors. The
assembly isn't going to be continuously flexed back and forth, it is
going to be formed in a fixture and remain that way and installed into
the upper-level assembly where it will stay in the formed position.
 
Should I do anything with it other than maybe carefully trim it off?
Will any repair actually do anything as far as reliability is concerned?
For that matter, has the tear compromised the reliability of the flex in
that area? There's been suggestions of some sort of epoxy repair, but I
don't think that it will buy you anything as far as reliability is
concerned.
 
What do you think I should do?
 
Steve Gregory

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2