TECHNET Archives

December 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Phil Bavaro <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 31 Dec 2013 17:25:46 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (73 lines)
This is a new one for me.   It appears to me that the panel has already been cut almost all the way through based on the cross section photo. It also appears that whatever cut it, went right through both copper and internal  fiberglass and epoxy.  Only the very last fiberglass material left in the middle appears to be holding it together.

At 1.24 mil wide, I don't see how any rolling mechanical blade will fit into the chasm between the two sides of the cut.

Without knowing the specifics of how this was manufactured, it looks like it is ready to be broken off as is.
I guess the real answer is to get back to the person who prepared this for you and ask them how they expected you to separate the boards.

If that is not possible, then I think Dean nailed it on his first answer.  Use your sharpest knife and steadiest operator to carefully follow the score line guide already provided.  Don't press too hard and make cuts from both sides, if necessary.

Phil


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Tuesday, December 31, 2013 8:23 AM
To: [log in to unmask]
Subject: Re: [TN] super fine score cuts

The caution with laser singulation is that the laser will carbonize the FR-4 along the edge. That is not a concern so long as the copper does not come out into that area.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, December 31, 2013 9:00 AM
To: [log in to unmask]
Subject: Re: [TN] super fine score cuts

Morning Guy,

Wow! 1.24 mil score! I wonder how that was done? Laser? Water-jet?
Here's the pictures:

http://stevezeva.homestead.com/micro_v-score.jpg

http://stevezeva.homestead.com/panel_edge_230x.jpg

From the panel edge photo, it looks like there's no "V" relief to allow for any sort of real singulation in the conventional way that you use a V-score.

Best has a laser that can be used to de-panel something like this:

http://www.solder.net/services/laser-services/

Steve

-----Original Message-----
From: Guy Ramsey [mailto:[log in to unmask]]
Sent: Tuesday, December 31, 2013 6:31 AM
To: Steve Gregory; 'TechNet E-Mail Forum'
Subject: super fine score cuts

Hi Steve,
We have a 3 inch square panel of 144 little boards. They have the finest little score cuts I have ever seen.
Each one has a tiny embedded device. I am afraid to break them apart.
Wondering if you can post the pictures, and if you or anyone on Technet has a good idea for how to singlulate the boards.

Thanks,
Guy


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
________________________________
 This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2