TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
X400-Content-Type:
P2-1988 ( 22 )
Old-Return-Path:
Date:
12 Dec 96 16:27:29 -0500
Precedence:
list
Resent-From:
Conversion:
Allowed
Disclose-Recipients:
Prohibited
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
From [log in to unmask] Fri Dec 13 12:
51:08 1996
X-Loop:
Content-Return:
Allowed
X-Mailing-List:
<[log in to unmask]> archive/latest/8523
TO:
"[log in to unmask]" <[log in to unmask]> (Return requested)
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vYL9U-0000UuC; Thu, 12 Dec 96 18:06 CST
Return-Path:
<TechNet-request>
X400-Originator:
X400-Recipients:
non-disclosure;
Alternate-Recipient:
Allowed
Message-Id:
<049EF32B078C1004*/c=us/admd=cwmail/prmd=carrier/o=syracuse/ou=ccmail1/s=Parr/g=Aric/@MHS>
Resent-Message-ID:
<"wzJwt3.0.8AA.Vu9io"@ipc>
Subject:
From:
"Aric Parr" <[log in to unmask]>
Priority:
non-urgent
X400-Received:
by /c=us/admd=cwmail/; Relayed; 12 Dec 96 16:27:29 -0500 by mta MTAwltk in /c=us/admd=cwmail/; Relayed; 12 Dec 96 16:27:29 -0500
Content-Identifier:
049EF32B078C1004
X400-Mts-Identifier:
[/c=us/admd=cwmail/; 049EF32B078C1004-MTAwltk]
Parts/Attachments:
text/plain (67 lines)

     no, your not.


______________________________ Reply Separator _________________________________
Subject: Re: (ASSEM) Wave soldering SOT-23
Author:  [log in to unmask] at internet
Date:    12/12/96 3:21 PM


> Tom:
>
> If you are using no-clean flux to solder SOTs (or anything with tall, 
> non-solderable body that will repel the wave from reaching the pad, 
such as
> tantalum capacitors), dual wave would not work. This is because the 
first
> wave (chip or turbulant wave) will kill the flux, resulting in the 
poor
> solderability at the second wave (lambda wave). The way we do it 
rather
> successfully is to elongate the pad size and solder them with a 
vibrating
> wave (omega wave), which has much lower surface energy to reach any 
shadowed
> pads. Good luck.
>
> Regards
> Jauwhei Hong
> [log in to unmask]
     
Jauwhei Hong,
We don't have any problems soldering SOT's with no-clean flux and 
dual-wave (chip & lambda). We get fine results if we only use an angle 
of 4 degrees, accurate dwell time for the specific pcb and a "perfect" 
preheat profile. We also don't have to elongate the pad sizes, we use 
the ordinary sizes the pick & place do.
     
i don't know, but are we different?
     
/Jan Merstrand
 Operation Engineer
 Ericsson Microwave Systems
 [log in to unmask]
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2