No specific alloy is "forbidden" in military electronics.
In general, solders and fluxes are categorized per and must comply with
J-STD-004, J-STD-005, and J-STD-006.
Specific solder alloy types are called out on assembly prints and BOMs
per MIL-STDs and Weapon Specs.
Military, traffic control, industrial safety, some medical, and many
other products are exempt per RoHS and IEEE exemptions.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave Dixon
Sent: Wednesday, September 12, 2007 8:33 AM
To: [log in to unmask]
Subject: Re: [TN] Military Exemption from Lead-Free?
Check out
Air Force's Airworthiness Advisory AA-05-01 It isn't very forceful in
the wording, but is the closest thing I could find so far to support my
cause. If anyone knows of any documentation forbidding lead free in
military products, I would sure appreciate a heads-up.
Thanks,
Dave
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of ekalgren
Sent: Tuesday, September 11, 2007 3:06 PM
To: [log in to unmask]
Subject: Military Exemption from Lead-Free?
I believe that I remember someone mentioning a military end-use
exemption from lead free requirements. Am I remembering correctly or is
this just wishful thinking? If it is true, can anyone point me in the
direction to get it in writing?
Thanks!
Eric Kalgren
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|