Sender: |
|
X-To: |
|
Date: |
Mon, 15 Oct 2007 09:25:57 -0500 |
Reply-To: |
|
Subject: |
|
From: |
|
Content-Transfer-Encoding: |
quoted-printable |
In-Reply-To: |
|
Content-Type: |
text/plain; charset="us-ascii" |
MIME-Version: |
1.0 |
Parts/Attachments: |
|
|
Morning Tom,
One thing might help is to go to the largest mesh size solder paste that
you can use, small mesh sized solder paste tend to have more fines and
oxidation that sometimes create solder balls that don't coalesce back
into the main fillet.
Kind regards,
Steve Gregory
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, October 12, 2007 4:17 PM
To: [log in to unmask]
Subject: Re: [TN] Small solder balls
Hi Tom!
Got your picture posted. It's at:
http://stevezeva.homestead.com/files/1206_SolderBall.JPG
What kind of soldermask is on the board? LPI or dryfilm? Do you have the
mask relieved around the pads by a few mils?
I ask that because it almost looks like the solderball is caught right
at the edge of the mask sort of...
Steve Gregory
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gervascio, Thomas
Sent: Friday, October 12, 2007 1:38 PM
To: [log in to unmask]
Subject: [TN] Small solder balls
Has anyone ever established a baseline of the anticipated frequency of
solder balls under chip components? We are doing Space assembly work and
the specifications allow for no solder balls. We are using a ROL0 solder
paste and cleaning in an inline semi-aqueous cleaner with
saponification. What is being rejected are solder balls about a 1-2 mils
in diameter that are intermittently trapped under low profile chip caps
and resistors. I suspect it is an agglomeration of solder particles in
the paste occurring during reflow. I have tried all the usual things-
stencil aperture modifications: - homeplates; reverse homeplates(like a
bowtie design that reduced the printed pad by 25%); homeplates which are
offset 7 mils from the inside edge of the pad: tried reducing hot slump
of the paste (changed from 90sec soak between 150-170 sec (per vendor
recommendations) to ramp to spike; tried reducing placement force or
fudging part thickness.
What I am experience I believe is typical of the process but would like
some input from my peers.
Steve Gregory, can I post a photo on your website- stevezeva.com to show
what I am talking about?
Thanks
Tom Gervascio
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|