TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Bev Christian <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Date:
Fri, 23 Sep 2005 16:06:38 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (119 lines)
Ioan,
Any chance the parts are MSL parts that were not properly stored and
handled and they have pop corned, resulting in broken bond wires that
are really, really close and when a temp change happens things touch.
The other suggestions have been good too.
Bev

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brinkman, Mark
Sent: September 23, 2005 3:59 PM
To: [log in to unmask]
Subject: Re: [TN] Soldering or design problem?

At this point I think I would try to isolate the problem by debugging
the failing board. The designer should be able to find what is not
working. He should know the sequence of events that should take place
once power is applied to get the design up and running. He's going to
have get dirty. Find the event that is not working. What would cause
this event not to happen? Find it and see if it's the same on the other
failed boards.

 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Friday, September 23, 2005 2:40 PM
To: [log in to unmask]
Subject: [TN] Soldering or design problem?

Hi Technos,

we are faced here with a very delicate problem: the customer suspects a
workmanship issue on our side, we are suspecting a design or component
problem.

Here it goes: 50% of the cards do not function due to the same problem,
something wrong with the same PBGA. We tweaked the thermal recipe, we
are at about 220C peak; no improvement. We played with lower
temperatures for fear not to thermally stress the part; no improvement.

Now I get into the weird zone:
*       if the BGA is heated, it instantly starts working, but also
starts working if the BGA is frozen
*       it also works if we freeze the opposite side of the PCB
*       We use the flying probe to test for open joints, everything
seems to be OK, but the card does not work
*       we did all kinds of re-reflow of the BGA on the bad boards, in
the oven, but also on the rework station, even at extreme temperatures
that send the top of the part at 280C. Same pattern, heat/freeze, it
works, ambient temperature - fail. So we didn't even manage to kill the
part for good.
*       we change the component, bingo, it works in 90% of the cases

I am sure the soldering is OK and the joints are properly formed, but
don't have a solid proof, for some people BGA soldering is still the
cause of all problems.

My question is: if it's not the soldering, what else can it be? Can an
electronic design be borderline so that it does not work with the first
time reflowed BGA, but works right after replacing the part with parts
from the same tray? Can something be in the design of the PCB, in the
manufacturing of the PCB?

And a last one, what is the test that can confirm the absence of open
joints under a BGA? Can the balls be cross-sectioned parallell with the
PCB, like half-ball, so an eventual open be redily spotted?

Thanks,
Ioan

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------




---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2