I did an experiment this morning. I put a couple of drops of flux on a penny
about three hours ago, and I just looked at it...green as grass. It was
Kester ZX-2331 WS
-Steve Gregory-
> There was some soldermask touch up but not anywhere near the parts in
> question. I am thinking that since the board was assembled in one area and
> bagged to bring it in for cleaning that there might have been some WS flux
> in
> the bag. That seems the most likely right now.
>
> -----Original Message-----
> From: Crepeau, Phil [mailto:[log in to unmask]]
> Sent: Wednesday, May 05, 2004 12:25 PM
> To: [log in to unmask]
> Subject: Re: [TN] Green residue.
>
>
> is there any chance there was solder mask touch up going on in this area?
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------