TECHNET Archives

December 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Collins Graham <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Collins Graham <[log in to unmask]>
Date:
Wed, 1 Dec 2004 09:12:51 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (229 lines)
I'd have said he's avionics related as he does spend a fair amount of
time jetting about.

regards,

Graham Collins
Process Engineer, 
Northrop Grumman Canada Corporation
Halifax
(902) 873-2000 ext 6215

>>> [log in to unmask] 12/01/04 09:56AM >>>
Not so.  Graham is hi-rel and so exempt from the EU legislation.

Doug Pauls



                                                                       
   
             "Whittaker, Dewey                                         
   
             (AZ75)"                                                   
   
             <Dewey.Whittaker@                                         
To 
             HONEYWELL.COM>            [log in to unmask]                 
   
             Sent by: TechNet                                          
cc 
             <[log in to unmask]>                                         
   
                                                                  
Subject 
                                       Re: [TN] VOCs                   
   
             12/01/2004 07:47                                          
   
             AM                                                        
   
                                                                       
   
                                                                       
   
             Please respond to                                         
   
              TechNet E-Mail                                           
   
                   Forum                                               
   
             <[log in to unmask]>                                         
   
             ; Please respond                                          
   
                    to                                                 
   
             "Whittaker, Dewey                                         
   
                  (AZ75)"                                              
   
             <Dewey.Whittaker@                                         
   
              HONEYWELL.COM>                                           
   
                                                                       
   
                                                                       
   




After reading the first paragraph, a few of us who know Graham are
concerned
he could be banned from the EU after July 2006.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Brian Ellis
Sent: Wednesday, December 01, 2004 5:37 AM
To: [log in to unmask] 
Subject: Re: [TN] VOCs


It also includes your breath after having partaken ¼ of a unit of any
alcoholic beverage, includin beer and wine.

As usual, the EU has, by its definition, demonstrated its habitual
scientific ineptitude. It takes no notice whatsoever of the effect a
VOC
has on the environment. Not all VOCs photoreact with NOxs in the same
way. The directive that Graham quotes applies particularly to
solvents.
Some alkane or alkene solvents, as well as most cyclic ones, react
severely, where others have hardly any effect. For example, "white
spirit" and terpenes are bad but perchloroethylene has almost no
effect,
but the permitted stack concentrations are identical for all of them.
Plumb crazy, again.

The US regulations and exemptions on VOCs depend largely on which
lobby
can cry the loudest, especially in CA.

On neither side of the Atlantic is the legislation based on sound
science. (Where have I heard that before?)

Brian

Graham Naisbitt wrote:
> David
>
> Fluxes are used for essentially 2 purposes: one to remove surface
oxides
and
> to facilitate good wetting and second as a heat transfer medium.
>
> You then ask: "do they burn off...during the soldering process" - to
quote
> my good friend Doug Pauls: "It depends".
>
> It depends on the type of flux being used. If it is a no-clean flux,
then
it
> is the flux manufacturers intention that the res
idues - and ALL
fluxes
leave
> residues - shall be volatilised off the surface by the correct amount
of
> heat relative to residue volume. Of course, if you have areas (i.e.
topside
> in wave soldering) that do not see the correct temperature for the
desired
> time, then they will remain behind and might cause you some
reliability
> issues when in the field.
>
> Some other rosin based, dare I say classic, fluxes, are sometimes
designed
> to be left on the surface, or at least may be left behind in the
knowledge
> and comfort (well, on a wing and a prayer sometimes!) that they will
be
> cleaned off afterwards.
>
> VOC's:
>
> As defined by ³Council Directive 1999/13/EC of 11th March 1999:
> 17. volatile organic compound (VOC) shall mean any organic compound
having
> at 293.15 K a vapour pressure of 0.01kPa or more, or having  a
corresponding
> volatility under the particular conditions of use
>
> As defined by ³Council Directive 1999/13/EC of 11th March 1999:
> Organic compound shall mean any compound containing Carbon and at
least
one
> or more of hydrogen, halogens, oxygen, sulphur, phosphorous silicon
or
> nitrogen
>
> As defined by ³Council Directive 1999/13/EC of 11th March 1999:
> 9. *emission shall mean any discharge of volatile organic compounds
from
an
> installation into the environment. *into air, soil and water as well
as
> solvents contained in any products. They include uncaptured
emissions
> released to the outside environment via windows, doors, vents and
similar
> openings.
>
> VOC Controls:
> USA = Tax on solvents BUT Tax-Free solvents on EPA list
> EU = Anything with a vapour pressure that is >0.01kPa @293.15K
> This includes Whisky, Gin, Brandy, Vodka*but not beer and wine!
>
> I hope this helps
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives 
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives 
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2