Genny,
I just had to change a nylon fitting because it's outgassing properties
were well above space requirements. Turned out that the type of Nylon
had a total mass loss (TML) level of 2.5%, almost 50% of which would be
water. Granted this is a space application, but it demonstrates how some
materials may perform in 0 G. Outgassing may not hurt my fitting, but
the vapors it releases may damage neighboring parts.
I can think that the connector would popcorn during soldering similarly
to plastic components.
Hope this helps. Good Luck
Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
Sent: Wednesday, May 13, 2009 2:43 PM
To: [log in to unmask]
Subject: [TN] Nylon connectors - moisture sensitivity
We have been told that a surface mount nylon connector we use is
moisture sensitive, and should be treated as equivalent to level 5a.
This is the highest level we have ever seen on any component we have
used of any type. I didn't think that a connector could be moisture
sensitive. Not heat tolerant, yes - we have melted a few - but moisture
sensitive?
What kind of damage can happen to a nylon connector from too much
moisture absorption?
Thanks in advance for your responses.
Genny
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|