Parts/Attachments:
text/plain (90 lines)
Jon,
While that is true, that only relates to the compatibility between fluxes. 
 Seldom do you have flux vendors also providing coatings.  It is the 
product of the combined flux residues with the coating, especially the 
solvent carrier, that you have to watch out for.

Doug Pauls



[log in to unmask] 
Sent by: TechNet <[log in to unmask]>
03/04/2010 03:00 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]


To
[log in to unmask]
cc

Subject
Re: [TN] Conformal Coat Over No-Clean Flux






 
 
In a message dated 3/4/2010 3:37:16 P.M. Eastern Standard Time, 
[log in to unmask] writes:

You've  got to make very sure that the solder wire's core-flux or the 
liquid
assist  flux plays well with the conformal coating and there are 
definately
combinations of fluxes and coatings that don't get along. 

---------------

One very good way to do that is to get the flux (or cored solder) and 
coating from the same manufacturer.  That way the manufacturer will 
certify  the 
compatibility of the two materials.
 
 
 
Jon Moore



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2