TECHNET Archives

April 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 18 Apr 2007 14:35:29 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (148 lines)
Joe the percipient sage, again. Damn straight answer. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Fjelstad
Sent: Wednesday, April 18, 2007 2:21 PM
To: [log in to unmask]
Subject: Re: [TN] NTC An alternate view on lead in solders

Hi John,
 
Based on the tone of the comments, I don't think it would help.    
 
Best, 
Joe     
-----Original Message-----
From: [log in to unmask]
To: [log in to unmask]
Sent: Wed, 18 Apr 2007 11:40 AM
Subject: [TN] NTC An alternate view on lead in solders


Hi Guys,

Here is an alternate viewpoint on lead in solders sent to me though the
site. Anyone want to educate Bill on the environmental aspects of this
be my guest I have copied him on this email.

Bill  - nice Loctite ad - do you work for them??

John

 
 
John Burke
 

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Wednesday, April 18, 2007 8:41 AM
To: [log in to unmask]
Subject: EasySiteWizard FORM (http://www.rohsusa.com/home.html)


FullName = Bill Fretts

EmailFrom = [log in to unmask]

Subject = Call the Waaambulance!

MyComment = Buck up you whiners and start solving problems.

 > Lead has to get out of ewaste. Much of the world is burning it for
energy
reclamation / landfill diversion and the effects of the airborne lead
needs
to be a factor in the analysis. Local North American dumps are planning
to
burn now too. Balance the odd h/w failure with the survival of the
species.

> Tin whiskers - are manageable but you need standards on lead finishes.
Consumer JEDEC parts don't care about whiskers since their stuff is
disposable or 5 year life. NT and others have very specific finish
specifications for their components to disqualify whisker prone finishes
-
bright tin & Bi in particular. Those tin whisker horror stories get
trotted
out every few years.

> Hi Rel or Extreme Service SAC Reliability is pretty good. The joints
are
more brittle, but they're stronger too. If its for high mechanical shock
service (automotive etc) look to the Locktite SAC solder flux /
underfill,
like peanutbutter for chocolate.


Loctite(r) 3536 delivers improved reliability for today's advanced CSP
and BGA
packages. The material is designed to quickly fill the space beneath the
CSP
and BGA packages and cures rapidly at low temperature, which minimizes
thermal stress to other components on the PCB and allows for in-line
curing
to increase device throughput. When fully cured, Loctite 3536 delivers
excellent protection for solder joints against mechanical stress such as
shock, drop and vibration in hand-held devices and testing confirms its
superiority over competitive materials when subjected to these stresses.
In
addition, testing of the material to JEDEC drop test standards on 0.4mm
and
0.5mm Pb-free devices has shown that Loctite 3536 offers five times the
reliability over non-underfilled Pb-free devices.

Xsubmit = Submit

 = 

----------------------------------------
[IP: 161.44.198.204]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------
________________________________________________________________________
AOL now offers free email to everyone.  Find out more about what's free
from AOL at AOL.com.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2