TECHNET Archives

April 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Kathy Kuhlow <[log in to unmask]>
Date:
Thu, 11 Apr 2002 08:15:01 -0500
Content-Type:
multipart/mixed; boundary="=_1D409970.1E7F12CA"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Kathy Kuhlow <[log in to unmask]>
Parts/Attachments:
text/plain (698 bytes) , TEXT.htm (1062 bytes)
I would look at the plastic construction and maybe go through the UL file requirements for that plastic.  They are probably the answer on what the flammability rating would be with data to support it.  Maybe looking at the UL tests you could find reasoning that your customer would accept.

Interesting problem though.  We don't currently have products were pin to paste is possible due to several factors so I have not had to look at components for this recommendation.  Are component manufacturer's testing and making recommendations for pin to paste processes (other than this part) or has the industry missed the boat and this will become a larger issue as the technology grows?  

Kathy 



<!DOCTYPE HTML PUBLIC "-//W3C//DTD HTML 4.0 Transitional//EN"> <HTML><HEAD> <META http-equiv=Content-Type content="text/html; charset=iso-8859-1"> <META content="MSHTML 6.00.2713.1100" name=GENERATOR></HEAD> <BODY style="MARGIN-TOP: 2px; FONT: 10pt MS Sans Serif; MARGIN-LEFT: 2px"> <DIV>I would look at the plastic construction and maybe go through the UL file requirements for that plastic.&nbsp; They are probably the answer on what the flammability rating would be with data to support it.&nbsp; Maybe looking at the UL tests you could find reasoning that your customer would accept.</DIV> <DIV>&nbsp;</DIV> <DIV>Interesting problem though.&nbsp; We don't currently have products were pin to paste is possible due to several factors so I have not had to look at components for this recommendation.&nbsp; Are component manufacturer's testing and making recommendations for pin to paste processes (other than this part) or has the industry missed the boat and this will become a larger issue as the technology grows?&nbsp; </DIV> <DIV>&nbsp;</DIV> <DIV>Kathy </DIV></BODY></HTML>