TECHNET Archives

April 2019

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jack Olson <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Jack Olson <[log in to unmask]>
Date:
Thu, 4 Apr 2019 10:00:43 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (12 lines)
On Thu, 4 Apr 2019 09:40:44 -0400, Yuan-chia Joyce Koo <[log in to unmask]> wrote:

>does your vendor got small plating tank that not suitable for your
>large panel? (insufficient stir or agitation?)
>just curious. (i know it kills the cat)
>jk

I visited there, and the panels are fully immersed,
but I got the impression that the plating is not even from one side to the other, (or from top to bottom maybe) 
so they flip it and plate again.
I didn't know if this was common practice for pattern plating. 