TECHNET Archives

April 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Hernefjord Ingemar <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Hernefjord Ingemar <[log in to unmask]>
Date:
Mon, 2 Apr 2007 09:24:52 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (26 lines)
 Hi all,
 
I have still questions about fine sand and dust on conformal coated
boards. We have boards spread around the world, some in regions with
sand storms, as I've mentioned in earlier mails. Anyone who knows how
the guys do in Iraq, to mention one example? Sand must be creeping in
everywhere. Do the guys take out the boards and brush off the sand, or
do they just let the sand be there? In theory, sand is oftenly silicon
and quarts products, and as such, sand on coated boards should not be a
problem, because the particles are nearly 'insulators'. There seem to be
various opinions. Some take out the boards regularly and clean them,
others mean that the sand does not harm. Would be interesting to hear
any experienced voice in this forum.

Inge

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2