Mime-Version: |
1.0 |
Sender: |
|
Subject: |
|
From: |
|
Date: |
Wed, 3 Feb 1999 19:12:51 -0500 |
Content-Type: |
text/plain; charset="us-ascii" |
Reply-To: |
|
Parts/Attachments: |
|
|
Group,
I am interested in wet etching sputtered copper on a semiconductor
wafer.
I realize that I'm not talking boards here, but I'm hoping that someone
can
give me some insight to the problems that I'm facing.
Using traditional positive photoresists for semiconductor manufacturing,
I
am getting a very large undercut of my copper features. Features are
4-8
mils in x,y and anywhere from a few thousand angstroms to 1 um thick.
Unfortunately, the amount of undercut is 10-20 times the feature
thickness.
(I would expect 1x the feature thickness) I believe the problem is the
interface between the copper and the resist. When I use a metal mask
(say
Al), no appreciable undercut is observed. Also, the undercut seems to
be
independent of etch solution. Right now I am using a dilute
sulfuric/peroxide mixture.
In the pcb world, I assume copper is etched with photoresist masks. The
question is, is the photoresist a different chemistry to improve the
adhesion/interface between the polymer and the copper? If so, what
photoresists exist out there? And finally, is there a version that can
be
applied by SPIN coating (i.e. semiconductor process)?
Any insight would be greatly appreciated!
Jeff
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|