Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0weMjA-000BkTC; Wed, 18 Jun 97 10:32 CDT |
Old-Return-Path: |
|
Date: |
Wed, 18 Jun 97 15:45:53 UT |
>From willli Wed Jun 18 10: |
33:14 1997 |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"tH-MC1.0.UXD.c-_fp"@ipc> |
Subject: |
|
From: |
|
Precedence: |
list |
X-Loop: |
|
From [log in to unmask] Tue Jun 24 14: |
02:08 1997 |
Message-Id: |
|
Parts/Attachments: |
|
|
We currently use tin as a primary etch resist and a nitric-acid based tin
stripper.
We are experiencing difficulties with waste treating the spent stripper:
* Tin is OK to go to drain, but NOT the copper. We would prefer to recover the
tin, also.
* Precipitation is possible but only after a 4:1 dilution recommended by the
vendor of the stripper and by vendors of flocculants which generates more
liquid waste.
* The precipitated tin is very fine, even with precipitation aids, and when
the precipitate enters the filter press, it clogs the press rapidly.
Are there any means or methods to accomplish waste treating nitric-acid based
tin strippers to recover the tin and to treat the copper? Any alternative
methods possible?
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|