Thanks for the info so far. Upon closer examination of the part numbers we
have in house, I noticed that the Teflon coated wire was a 19 strand type,
while the PVC coated wire was a 7 strand type. Would these finer strands
also make the wire much more susceptible to breakage with a little wiggling
(the initial problem)? Do you think that if I brought in a 7 strand teflon
coated wire that it might solve some of the breakage problems?
Thanks.
-----Original Message-----
From: Genny Gibbard [mailto:[log in to unmask]]
Do you remember my question regarding the midplane assembly?
Turns out that there was a reel of mislabelled wire in house, and a whole
bunch of assembly has been done using a PVC coated wire, instead of the
teflon coated wire I spec'd. Apparently the wire in question is obsolete,
but they like using it better than the teflon, and want to continue to use
that.
I don't know much about wire coatings - what is the difference between these
two coating types, and when would you want to or not want to use them. I
need to decide whether we need to force them to change out the wiring
they've already done.
Sigh...
Thanks for your help in advance.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|