TECHNET Archives

April 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Hernefjord Ingemar <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Hernefjord Ingemar <[log in to unmask]>
Date:
Mon, 16 Apr 2007 11:05:56 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (61 lines)
Adam,

Clark pumps use SS for this fluid, as it seems.
Inge

http://www.clarksol.com/html/GearPumpMatCompat.htm


How are you these days, Brian? As an arbiter elegantum, I suppose you
live a calm and comfortable life nowadays. Don't see you as freq as
usual online.

Inge

 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Adam Seychell
Sent: den 16 april 2007 09:53
To: [log in to unmask]
Subject: [TN] stainless compatibility in alkaline etchant

Does anyone know if stainless steel 316 corrodes when exposed to
alkaline ammonia chloride etchants ?  I have this diaphragm pump with
internal stainless steel fasteners which are exposed to the etchant. The
pump elastomers are EPDM and santoprene, and body material is glass
filled polypropylene. I am wondering if the pump can be used for
alkaline etchants.

For a test I placed some stainless steel in etchant at let standing for
one week. There was no visible surface corrosion, nor any measurable
mass loss. I know this doesn't tell me I can use the pump and expect it
to last.


best regards,
Adam Seychell

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2