In a heat-transfer program, I use 112 lbm/ft^3 (1.79 g/cc) for FR-4 B-stage epoxy but I forget my source.
...and I have 1.82 SG (1.82 g/cc, 113.6 lbm/ft^3) for NEMA FR-4 laminate from the Modern Plastics Ency. '86-'87.
J. Felts
-----Original Message-----
From: Pucket, Larry Lee [SMTP:[log in to unmask]]
Sent: Tuesday, March 02, 1999 9:58 AM
To: [log in to unmask]
Subject: [TN] FR4 Density
Looking for the density of FR4 material in grams/cc.
Thanks in advance.
Larry Pucket
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|